Lubricant Additives & Plastic Stabilizers: Triphenyl Phosphorothioate (TPPT, CAS 115-86-6) is Sinolook's dual-application specialist - the only product in the range that serves simultaneously as a high-performance lubricant additive (AW/EP/AO) and as a polymer heat stabilizer (PVC, PP, PE secondary stabilization). This dual functionality stems from its core chemistry: the (PhO)₃P=S molecular structure - three phenoxy ester groups on phosphorus, with a P=S thione function. In tribological applications, the P–S and P–O bonds undergo thermally and tribologically activated surface chemistry, forming iron phosphate/iron sulphide composite tribochemical films for AW/EP protection, while the thione sulphur provides radical scavenging AO activity. In polymer processing, the same P=S function acts as a peroxide decomposer (secondary antioxidant mechanism), intercepting alkyl radicals and hydroperoxides that initiate thermal degradation of PVC, PP, and PE at processing temperatures (150–220°C). TPPT is also notable as the only solid (crystalline powder, MP 56–58°C) AW/EP additive in the Sinolook lubricant range - all others are liquids. This requires attention to dissolution approach but enables precision dosing by weight and easy incorporation into solid formulations. Sinolook Organophosphorus Series: TPPT CAS 115-86-6 (this).
★ DUAL USE: Lubricant AW/EP/AO + PVC/PP/PE Stabilizer · Solid Crystalline Powder · Purity ≥99.0% · MP 56–58°C · P ~9% · S ~9.4% · Ash ≤0.01% · Zero Metals · (PhO)₃P=S · MW 342.35 · CAS 115-86-6
Triphenyl Phosphorothioate (TPPT)
TPPT / Triphenyl Thiophosphate / Phosphorothioic Acid, O,O,O-triphenyl ester / 硫代磷酸三苯酯 / CAS 115-86-6 / (PhO)₃P=S / MW 342.35 g/mol / White Crystalline Solid / Purity ≥99.0%
| CAS Number | 115-86-6 |
| Structure | (PhO)₃P=S / O,O,O-Triphenyl phosphorothioate. Three phenoxy (–O–C₆H₅) groups attached to tetravalent phosphorus, with a P=S thione double bond. Molecular formula: C₁₈H₁₅O₃PS, MW 342.35. The P=S bond (BDE ~335 kJ/mol) is the key reactive bond - tribochemical activation cleaves it to release reactive phosphorus and sulphur species. Image skeletal formula: P(centre) = S(yellow, below), three –O–Ph arms. 3D model: yellow = S (P=S thione sulphur); red = O (three ester oxygens); black = C; white = H. No blue N, no grey Mo, no green B - confirming pure P/S organophosphorus chemistry with no metals. |
| ★ Physical form | ⚠ SOLID - White to pale yellow crystalline powder (MP 56–58°C)
The only solid AW/EP additive in the Sinolook lubricant range. Melts cleanly at 56–58°C. Dissolution method: pre-melt at 60–70°C and add to warm base oil (>60°C) with stirring, or dissolve directly in aromatic solvent carrier (toluene, xylene) then blend. In lubricant blending: add at oil temperature >65°C for direct dissolution. In plastic compounding: add as powder to the polymer/stabiliser blend before extrusion/calendering. |
| ★ Dual applications |
① Lubricant: AW + EP + AO ② Polymer: PVC/PP/PE secondary heat stabiliser
|
| SAPS Status |
⚠ P ~9.0% - phosphorus (manage ACEA P budget) ⚠ S ~9.4% - sulphur (manage ACEA S budget) ✅ ASH ≤0.01% - virtually zero ash (no metals) ✅ ZERO METALS - no Zn, no Mo, no Ca (unlike ZDDP and detergents)
TPPT: P+S double contribution (both SAPS elements) but virtually ash-free. At 0.3 wt% treat: P contribution ~0.027%, S contribution ~0.028%, ash ~0.00003%. Compare ZDDP: at equal treat rate P ~0.04%, S ~0.03%, ash ~0.04–0.06% (Zn). For ash-sensitive ACEA C1 (ash ≤0.5%), TPPT's near-zero ash leaves more headroom than ZDDP despite similar P/S at equal treat rate. |
| ★ Purity | ≥ 99.0% - pharmaceutical/reagent-grade purity
Highest purity of any additive in the Sinolook lubricant range. ≥99.0% (GC or HPLC) ensures maximum performance per gram, minimal unwanted by-product chemistry, and suitability for polymer-grade plastic stabiliser use where impurities can affect colour/clarity of the finished article. |
TPPT Mechanisms - Tribochemical AW/EP Film, Radical-Scavenging AO, and Polymer Thermal Stabilisation
Triphenyl Phosphorothioate (CAS 115-86-6) is one of the most compositionally pure and chemically well-defined AW/EP/AO additives in the lubricant industry. Its (PhO)₃P=S structure contains three phenyl ester arms and a single P=S thione - clean, symmetric, and with no metal impurities, no alkyl variability (unlike ZDDP where primary/secondary alkyl chains change reactivity), and no extraneous functional groups. This structural clarity gives TPPT highly predictable tribochemical behaviour and makes it the preferred choice when precise additive chemistry is required: polymer compounding (where colour, clarity, and regulatory compliance of stabiliser chemistry are critical), high-purity lubricant formulations, and applications where ZDDP's zinc ash is undesirable.
Under boundary lubrication (contact temperature 120–300°C, pressure >0.5 GPa), the P=S bond in TPPT undergoes tribochemically activated homolysis. The liberated reactive phosphorus species (phosphoryl/metaphosphate intermediates) react with the iron/steel surface to form an amorphous iron polyphosphate tribochemical film - structurally similar to the ZDDP-derived film but without zinc. This phosphate film (~10–50 nm thick) provides load-bearing AW protection: it is harder than iron, is self-renewing from TPPT reservoir in the lubricant, and has a lower friction coefficient than bare steel contact.
Simultaneously, the P=S sulphur - released more energetically under high-severity contact - reacts with iron to form a FeS / Fe₃O₄ composite EP film. This film provides extreme-pressure protection: FeS has low shear strength (preventing welding/scuffing) while Fe₃O₄ provides hardness and load support. The combination of iron phosphate (AW layer) + FeS (EP layer) gives TPPT its dual AW/EP character - a composite film functionally analogous to ZDDP's polyphosphate glass pad but with different elemental composition (P+S, no Zn). ASTM D2783 Weld Load: TPPT at 1.0 wt% in mineral base oil typically achieves Weld Load of 200–315 kg, documenting genuine extreme-pressure capacity.
The P=S thione sulphur in TPPT has an available lone pair that can donate H (from adjacent C–H) to peroxyl radicals (ROO•): P=S + ROO• → P=O + RS• → stable products. This makes TPPT a primary antioxidant (radical scavenger) through S-centred radical chemistry - analogous to thioester AOs (e.g. DLTDP) but with the P=S function providing the active site. The three phenyl rings also provide mild aromatic π-radical stabilisation. Combined P+S AO chemistry makes TPPT more effective as an antioxidant than simple phosphate esters (no S) or simple thioethers (no P).
The trivalent phosphorus equivalent (from P=S → P after sulphur loss) acts as a Lewis base toward hydroperoxides (ROOH), catalysing their decomposition to non-radical products: (PhO)₃P + ROOH → (PhO)₃P=O + ROH. This secondary AO mechanism is identical to the mechanism of triphenyl phosphite (TPP, (PhO)₃P), which is a well-known polymer antioxidant - TPPT's P=S generates a P(III)-equivalent in the oil under partial oxidation conditions, giving this secondary AO activity. Combined primary (S-based radical scavenging) + secondary (P-based ROOH decomposition) AO makes TPPT a genuine dual-function AO - unusual among AW/EP additives.
PVC thermal degradation during processing (160–200°C, calendering/extrusion) proceeds via HCl elimination from C–Cl bonds, creating polyene sequences that discolour the polymer (yellowing → browning → blackening). Primary Ca/Zn stabilisers absorb HCl by reacting with carboxylate ligands. TPPT acts as a secondary co-stabiliser: (1) its phosphorothioate function decomposes polyene peroxides that form during degradation; (2) it quenches Cl• and alkyl radicals formed in the HCl elimination cascade; (3) the phenoxy groups provide antioxidant protection against oxidative crosslinking. Together with Ca-Zn primary stabiliser, TPPT at 0.1–0.5 phr extends the thermal stability window of PVC by 10–30 minutes at 180°C (Congo Red test), enabling longer processing runs and more consistent product colour.
In polyolefin processing (PP/PE extrusion, injection moulding at 200–260°C), TPPT functions as a secondary processing antioxidant (analogous to phosphite antioxidants like Irgafos 168 but with additional S-AO function). The P(III) equivalent from partial P=S oxidation decomposes hydroperoxides (ROOH) formed by melt-phase oxidation: (PhO)₃P=S + ROOH → (PhO)₃P=O + S + ROH. This prevents melt discolouration, molecular weight degradation, and surface defects in PP/PE articles. Typical treat rate: 0.05–0.2 phr in combination with primary hindered phenolic AO (e.g. Irganox 1010/1076 equivalents). The ≥99.0% purity of TPPT ensures minimal impact on polymer colour - impurities (such as triphenyl phosphate or hydrolysis products) in lower-purity grades can cause yellowness index (YI) increase in transparent polymer applications.
| Property | ZDDP (Primary C8) | ★ TPPT (CAS 115-86-6) |
|---|---|---|
| Physical form | Amber liquid | ★ White crystalline solid (MP 56–58°C) |
| Purity | ~95%+ (variable) | ★ ≥99.0% (precise) |
| ★ Ash content | ~0.04–0.06% (Zn) | ✅ ≤0.01% - Near zero |
| Metals | Zn (~9%) | ✅ Zero metals |
| P content | ~10–12% | ~9.0% (similar) |
| S content | ~15–17% | ~9.4% (lower S) |
| ★ Polymer use | Not applicable | ★★ PVC/PP/PE stabiliser |
| AW tribofilm | Zn polyphosphate glass | Fe phosphate + FeS composite |
| ★ Physical form | White to pale yellow crystalline powder |
| ★ Purity | ≥ 99.0% |
| ★ Melting Point | 56–58°C (ASTM E794) |
| Molecular Formula | C₁₈H₁₅O₃PS · MW 342.35 |
| ⚠ P content | ~9.0 wt% (calc. from MW) |
| ⚠ S content | ~9.4 wt% (calc. from MW) |
| ✅ Ash content | ≤ 0.01% (near zero) |
| Acid Value | ≤ 0.1 mg KOH/g |
| ⚠ Moisture | ≤ 0.05% (KFT) |
| Solubility | Benzene, toluene, mineral oil, PAO; insoluble in water |
| Shelf life | 24 months (sealed, 5–25°C) |
Technical Specification
Highest in Sinolook range. Enables polymer-grade application (PVC/PP/PE stabiliser where impurities affect colour/clarity). Precise AW/EP performance per gram.
Only solid in Sinolook FM/AW range. Dissolve at >65°C in oil before addition to base formulation. Precise, crystalline - no batch-to-batch viscosity variability vs liquid additives.
Near-zero ash - no metallic residue. No Zn (unlike ZDDP), no Ca (unlike detergents). Maximum ACEA ash budget preserved for other components. Critical for polymer applications (no metal ash in plastic article).
Very low acid value confirms purity and hydrolytic stability. Acid value >0.1 indicates partial hydrolysis or impurities - measure at incoming QC to verify storage integrity.
Tighter moisture spec than TEGMEB (0.10%) - TPPT is a solid and more prone to caking/bridging if moisture-absorbed. Sealed packaging critical; silica gel desiccant bags in drums recommended.
| Parameter | Specification | Test Method | Technical Note |
|---|---|---|---|
| Appearance | White to pale yellow crystalline powder | Visual / ASTM D156 | Pale yellow tint acceptable. Brown/grey colour or strong odour indicates degradation or impurity. Free-flowing powder with no caking - caking indicates moisture absorption; test KFT immediately. |
| ★★ Purity | ≥ 99.0% | GC area % or HPLC | Primary QC parameter. Main impurities at <1%: triphenyl phosphate (TPP, no S), diphenyl phosphate, or oxidation products. GC confirms TPPT retention time. Polymer-grade applications require ≥99.0% to avoid discolouration in transparent PVC/PP. |
| ★ Melting Point | 56–58°C | ASTM E794 / DSC | Sharp MP (1–2°C range) confirms purity ≥99.0%. Broad MP range (e.g. 50–60°C) suggests impurities. Dissolves cleanly above 60°C - no decomposition up to 200°C. Handle as solid below 55°C; liquid above 60°C. |
| ✅ Ash Content | ≤ 0.01% | ASTM D482 | Near-zero ash - no metallic residue. B₂O₃/ZnO/CaO = 0. Minimum ACEA ash impact at any lubricant treat rate. Enables use at higher treat rates in ash-limited ACEA C1/C2 formulations vs ZDDP or detergents. |
| ⚠ Phosphorus (calc.) | ~9.0 wt% | Calc. from MW (31/342.35) / ICP-OES D5185 | P contributes to ACEA/API P limit. At 0.3 wt% treat: ~0.027% P in oil. Manage alongside ZDDP P contribution in ACEA C1/C3 engine oils. |
| ⚠ Sulphur (calc.) | ~9.4 wt% | Calc. from MW (32/342.35) / D4294 / ICP | S contributes to ACEA S limit. At 0.3 wt%: ~0.028% S. TPPT S is lower than ZDDP (~15–17%) - lower S SAPS impact per AW/EP equivalent. However S in TPPT is P=S thione (less reactive than active sulphur EP compounds, so lower copper corrosion risk). |
| Acid Value | ≤ 0.1 mg KOH/g | ASTM D974 | Very low acid value confirms intact P=S and P–O–Ph ester bonds. Acid value increase in stored product indicates hydrolysis - reject lot if acid value >0.5. |
| Moisture Content | ≤ 0.05% | Karl Fischer | Tightest moisture spec in Sinolook range. Solid form absorbs atmospheric moisture - store in sealed HDPE/metal drums with desiccant bags. Do not store in open containers. Caking = moisture indicator. |
| Packaging | 25 kg HDPE lined fibre drum or paper bag · 500 kg ton bags | - | 24-month shelf life sealed at 5–25°C. Stack ≤5 layers. Keep dry; no humidity >70% RH. Inner HDPE liner in fibre drum prevents moisture ingress. |
Applications & Dosage Guidance
1. Lubricant Additives - Engine, Gear & Hydraulic Oils
In engine oils (ACEA C1–C3, API SP), TPPT at 0.2–0.5 wt% provides AW/EP/AO performance as a ZDDP supplement or partial replacement in metal-sensitive or ash-critical formulations. The near-zero ash (≤0.01%) means that replacing 0.3 wt% ZDDP with 0.3 wt% TPPT reduces sulphated ash by ~0.015–0.020 percentage points - a meaningful contribution in ACEA C1 (ash ≤0.5%) where every 0.01% of ash headroom has value for other formulation components (detergents, VIs). For industrial gear oils (DIN 51517-3 CLP) and hydraulic oils (DIN 51524-2/3 HLP), TPPT at 0.5–1.5 wt% delivers excellent AW/EP protection - ASTM D2783 Weld Load >200 kg at 1.0 wt% - with non-corrosive copper behaviour (ASTM D130 1a–1b, as the P=S thione is a non-active sulphur type that does not corrode copper at normal treat rates). TPPT's solid form enables precise dose-by-weight incorporation, which is advantageous in continuous blending operations with loss-in-weight feeders or when tight P/S budget management per batch is required.
2. PVC Secondary Heat Stabiliser
TPPT is a well-established secondary heat stabiliser for PVC, used at 0.1–0.5 phr (parts per hundred resin) in combination with calcium-zinc (Ca-Zn) or barium-zinc (Ba-Zn) primary stabilisers. In rigid PVC (window profiles, pipes, fittings - ISO 15013/DIN 8061), TPPT at 0.2–0.3 phr combined with Ca-Zn 2.0–3.0 phr improves: (1) thermal stability time (Congo Red test at 180°C: +10–20 min extension vs Ca-Zn alone); (2) initial colour - TPPT's peroxide-decomposing function reduces yellowing immediately after processing; (3) long-term stability - prevents the "zinc burning" (sudden blackening) that occurs when Zn stearate is consumed by intercepting radical intermediates before irreversible discolouration. For flexible PVC (cables, hose, flooring), TPPT at 0.1–0.3 phr in Ca-Zn/Ca-Mg/epoxy plasticiser stabiliser systems improves wire & cable insulation heat stability ratings (IEC 60811 thermal aging resistance). The ≥99.0% purity grade is essential for transparent and food-contact-adjacent PVC formulations where lower-purity grades may introduce colour bodies from impurities.
3. PP/PE Processing Antioxidant (Secondary AO)
In polyolefin processing (polypropylene and polyethylene), TPPT functions as a secondary processing antioxidant alongside hindered phenolic primary AOs. The established industry standard for PP is a combination of primary AO (e.g. Irganox 1010, a phenolic pentaerythritol tetra-ester AO equivalent) and secondary AO (typically Irgafos 168, a phosphite triester). TPPT at 0.05–0.15 phr serves a similar secondary AO role as Irgafos 168-type additives, with the additional S-AO function from the P=S thione providing extra protection during high-temperature melt processing (>230°C, multi-pass extrusion). In polypropylene film (BOPP, BOPE), the Yellowness Index (YI) of the finished film is directly controlled by the secondary AO quality - TPPT at ≥99.0% purity maintains YI ≤2 in standard 0.05 mm BOPP film vs YI >5 observed with lower-purity phosphorothioate grades. For PE pipe (PE-RT, PE-HD water and gas pipe per EN 12201 / ISO 4427), TPPT 0.05–0.10 phr combined with phenolic AO meets long-term thermal oxidative induction time (OIT) requirements (>20 min OIT at 200°C, EN 728).
4. Metalworking Fluids & Specialty Lubricants
In oil-based metalworking fluids (neat cutting oil, ISO 6743-7 MH) and stamping/drawing oils, TPPT at 0.5–2.0 wt% provides combined AW/EP/AO protection. The iron phosphate + FeS composite film from TPPT tribochemistry performs well in high-speed steel and carbide cutting tool contacts - the non-active-sulphur character of P=S thione (compared to active sulphur polysulphides) means TPPT gives D130 copper corrosion 1a–1b, allowing its use in copper-alloy machining fluids where active-sulphur compounds are excluded. For hydraulic fluids in steel mill and marine hydraulics where fire-resistant phosphate ester fluids (HFD-R type) are used, TPPT can be added as a supplementary AW/AO additive - the phenoxy ester structure of TPPT is structurally compatible with phosphate ester base fluids, unlike sulphur-EP additives that can cause phase separation or reactivity issues in phosphate ester systems.
| Application | Treat Rate | SAPS note | Key Performance / Standard |
|---|---|---|---|
| Engine oil (ACEA C1–C3 AW supplement) | 0.2–0.5 wt% | P+S; ash ≤0.01% ✅ | Ash-free AW/AO; near-zero ash headroom vs ZDDP; RPVOT +300–500 min at 0.3 wt% |
| Industrial gear oil (CLP EP) | 0.5–1.5 wt% | P+S; ash ≤0.01% ✅ | D2783 Weld Load >200 kg; D130 1a–1b; DIN 51517-3 CLP; Cu-alloy safe (non-active S) |
| Hydraulic oil (HLP/HVLP) | 0.3–1.0 wt% | P+S; ash ≤0.01% ✅ | DIN 51524-2/3; D130 1a–1b; AW protection without Zn metal ash |
| PVC heat stabiliser (rigid: window/pipe) | 0.2–0.5 phr | Polymer grade | With Ca-Zn primary; Congo Red +10–20 min; initial colour improvement; purity ≥99.0% for transparent PVC |
| PVC heat stabiliser (flexible: cable/hose) | 0.1–0.3 phr | Polymer grade | With Ca-Zn/epoxy; IEC 60811 thermal aging resistance; fire-retardant flexible PVC formulations |
| PP/PE processing AO (secondary) | 0.05–0.2 phr | Polymer grade | With Irganox-type primary AO; YI ≤2 BOPP film; EN 728 OIT >20 min; multi-pass extrusion stability |
| Oil-based MWF (neat cutting/stamping) | 0.5–2.0 wt% | P+S; ash ≤0.01% ✅ | ISO 6743-7 MH; D130 1a–1b; Cu-alloy/bronze-safe; compatible with phosphate ester hydraulic base fluids |
Frequently Asked Questions
Q: TPPT is a solid. How do I incorporate it into lubricant oil blends?
TPPT's solid form (MP 56–58°C) requires one of three approaches: (1) Direct dissolution in hot base oil: heat the blending vessel or base oil to 65–70°C (above MP) with agitation, then add TPPT powder slowly. TPPT dissolves cleanly and completely in mineral oil, PAO, and ester base oils at ≥65°C within 15–30 minutes with stirring. The resulting clear solution remains stable on cooling (no precipitation at ambient temperature at typical treat rates of ≤2.0 wt%). (2) Pre-melt and addition as liquid: melt TPPT in a heated vessel at 65–70°C, then add the molten TPPT to the base oil while warm - this approach speeds dissolution and is preferred for large-batch blending. (3) Concentrate approach: dissolve TPPT in a compatible carrier (toluene, xylene, or a light mineral oil at elevated temperature) to create a 30–50 wt% concentrate, which can then be added to the final blend at ambient temperature. For plastic compounding (PVC/PP/PE), TPPT powder is added directly to the premix at the weighing stage - no pre-melting required as the extruder/calender temperatures (160–260°C) are far above the MP, ensuring complete incorporation.
Q: Does TPPT cause copper corrosion? The sulphur content concerns me.
TPPT contains ~9.4% sulphur as a P=S thione bond - this is non-active sulphur (chemically unreactive toward copper under standard lubricant conditions), which fundamentally differs from active sulphur compounds such as sulphurised esters or polysulphides. Active sulphur refers to elemental sulphur, H₂S, or sulphur released as reactive S• radical from thermally labile S–S or S–C bonds at <100°C. TPPT's P=S bond requires significantly higher temperatures and tribological activation (>120°C, high contact stress) for S release - under standard ASTM D130 copper strip test conditions (100°C, 3 hours), the P=S bond is not activated to release reactive sulphur. Consequently, TPPT at standard treat rates (0.5–1.5 wt%) typically achieves ASTM D130 copper strip rating of 1a–1b (no corrosion to slight tarnish) - comparable to ZDDP (typically 1b–2a) and far better than active-sulphur EP additives (typically 3c–4c). This non-corrosive character makes TPPT suitable for copper-alloy-containing systems (brass bushings, bronze bearings, copper brake lines) where active-sulphur EP additives are excluded.
Q: What is the difference between TPPT and regular triphenyl phosphate (TPP) as lubricant additives?
Triphenyl phosphate (TPP, (PhO)₃P=O, CAS 115-86-6 is TPPT while TPP is CAS 115-86-6 - note: these CAS numbers are distinct) and Triphenyl Phosphorothioate (TPPT, (PhO)₃P=S, CAS 115-86-6) are structurally related but differ by the substitution of S for O in the central double bond (P=S vs P=O). This single substitution makes a significant performance difference: TPPT has better AW/EP performance than TPP because the P=S bond is more reactive tribochemically (lower BDE ~335 vs P=O ~540 kJ/mol) - it decomposes more readily at contact surfaces to generate the tribochemical film; TPPT has significantly better AO performance than TPP because the thione sulphur participates in radical scavenging - TPP has no S-AO mechanism; TPPT has better thermal stability in polymer applications than simple phosphate ester plasticisers at melt-processing temperatures because the P=S function stabilises the molecule against hydrolysis and oxidative P=O conversion during compounding. TPP is primarily a flame retardant and plasticiser for PVC; TPPT is primarily an AW/EP/AO additive and heat stabiliser co-agent. In lubricant formulations, TPPT is preferred over TPP for AW/EP applications; in PVC, both have roles but with different primary functions.
Technical & Regulatory References
GC / HPLC (purity ≥99.0%) · DSC / E794 (MP 56–58°C, purity indicator) · ASTM D974 (acid value ≤0.1) · ASTM D482 (ash ≤0.01%) · KFT (moisture ≤0.05%) · ICP-OES D5185 (P ~9%, S ~9.4%) · ASTM D2783 Four-Ball EP (Weld Load / LWI) · ASTM D4172 Four-Ball Wear (WSD) · ASTM D130 Copper Corrosion (target 1a–1b) · ASTM D2272 RPVOT (AO performance) · Polymer: Congo Red test (PVC thermal stability) · EN 728 OIT (PE pipe AO performance) · YI ASTM E313 (film colour) · IEC 60811 (cable thermal aging)
Lubricants: ACEA C1/C2/C3 (P/S budget managed; ash ≤0.01% - minimum ash impact) · API SP/SN+ · DIN 51517-3 CLP · DIN 51524-2/3 HLP · ISO 6743-7 MH (MWF) · MIL-PRF phosphate ester compatible · PVC rigid: ISO 15013 (profile) · DIN 8061 (pipe) · EN 1557 (fitting) · EU RoHS (TPPT is RoHS compliant - no restricted metals) · REACH (verify annex XIV/XVII status for specific PVC applications) · PVC flexible / cable: IEC 60332 (fire) · IEC 60811 (thermal) · EN 50363 · PP/PE: EN 728 (OIT PE pipe) · ISO 4427 (PE water pipe) · EN 12201 · Food-adjacent PVC: Verify specific EU Regulation 10/2011 compliance per formulation
CAS 115-86-6 · EINECS 204-112-2 · REACH pre-registered (verify SVHC status: check current SVHC candidate list for organophosphorus esters with specific structural features) · TSCA listed · ⚠ P ~9.0% and S ~9.4%: contribute to ACEA/API P and S limits - calculate at treat rate · ✅ Ash ≤0.01%: virtually ash-free · FP above 160°C (estimated from solid MP; melt FP): non-flammable · GHS SDS: GHS08 (harmful if swallowed, organophosphorus compound - standard PPE: gloves, goggles, dust mask; avoid powder inhalation; organophosphorus acetylcholinesterase inhibition risk with high-dose exposure - standard industrial hygiene precautions) · RoHS compliant (no restricted metals) · For PVC food-contact applications: verify compliance with EU Regulation 10/2011 specific migration limits for the specific migration conditions
AW/EP/FM Additives: MoDTP ✅ · MoDTC ✅ · Mo Amine Complex ✅ · TEGMEB (Borate Ester EP) ✅ · TPPT CAS 115-86-6 ✅ (this) → ZDDP AW/AO ✅: Full range (Primary C4/C8 · Hybrid · Secondary-Primary Blend) → Phenolic AO ✅: BHT · DTBP · HP-136/L01/L57 → Amine AO ✅: ADPA · NDPA → Detergents/Dispersants ✅
TPPT · CAS 115-86-6 · (PhO)₃P=S · Purity ≥99.0% · MP 56–58°C · Ash ≤0.01% · AV ≤0.1 · Moisture ≤0.05% · P ~9% · S ~9.4% · White Crystalline Powder · 25 kg Drum/Bag · Lubricant AW/EP/AO + PVC/PP/PE Stabiliser
Request Pricing, Technical Datasheets & Application Guidance
Specify application: lubricant (engine/gear/hydraulic/MWF - provide treat rate target and ACEA P/S/ash budget) or polymer (PVC rigid/flexible, PP/PE - provide polymer type, processing temperature, and primary stabiliser system). Sinolook provides: GC/HPLC purity-confirmed COA; DSC melting point verification; copper corrosion D130 data; ASTM D2783 EP Weld Load data; PVC Congo Red stability test results; PP OIT data. Samples (1–10 kg) for formulation evaluation in lubricants or polymer compounds.
AW/EP/FM & Stabiliser Range:
MoDTP · MoDTC · Mo Amine Complex · TEGMEB · TPPT CAS 115-86-6 ✅ (this) → ZDDP ✅ · Phenolic AO ✅ · Amine AO ✅ · Detergents ✅
Hot Tags: triphenyl phosphorothioate, China triphenyl phosphorothioate manufacturers, suppliers, modtc oil additive